CHEMISTRY | X-SBR LATEX |
SOLID CONTENT | 49-50 |
VISCOSITY | 100-300 |
MFFT | 68 |
PH | 7.5-8.5 |
FILM HARDNESS | Hard |
Chemistry | X-SBR LATEX |
viscosity | 100-300 |
Solid Content | 49-50 |
PH | 7.5-8.5 |
MFFT | 45 |
Film Hardness | Hard |
dipping of non woven and back Coating of carpet
Chemistry | X-SBA LATEX |
viscosity | 100-500 |
Solid Content | 49-50 |
PH | 7.5-8.5 |
MFFT | >0 |
Film Hardness |
high adhesion to synthetic fibers , tacky dry film
Chemistry | X-SBR LATEX |
viscosity | 100-500 |
Solid Content | 49-50 |
PH | 7.5-8.5 |
MFFT | 25< |
Film Hardness | medium to hard |
excellent water resistance,good filer load ability
Chemistry | X-SBR LATEX |
viscosity | 200-900 |
Solid Content | 49-50 |
PH | 7.5-8.5 |
MFFT | >0 |
Film Hardness | very Soft |
modification of anionic emulsion bitumen.crack resistance in low temperature and flow resistance in high temperature
Chemistry | X-SBR LATEX |
viscosity | 100-500 |
Solid Content | 49-50 |
PH | 7.5-8.5 |
MFFT | 25< |
Film Hardness | Medium |
good filler load ability excellent water resistant , dipping and back coating technic
Chemistry | X-SBR LATEX |
viscosity | 200-900 |
Solid Content | 49-50 |
PH | 7.5-8.5 |
MFFT | 0 |
Film Hardness | Very Soft |
high filler load ability, excellent water resistant , dipping and back coating technic
Chemistry | X-SBR LATEX |
viscosity | 100-300 |
Solid Content | 49-50 |
PH | 7.5-8.5 |
MFFT | 68 |
Film Hardness | Hard |
heat forming textiles , excellent water resistant , dipping and back coating technic
Chemistry | X-SBR LATEX |
viscosity | 100-400 |
Solid Content | 49-50 |
PH | 7.5-8.5 |
MFFT | 58 |
Film Hardness | Hard |
heat forming textiles , excellent water resistant , dipping and back coating technic
Chemistry | X-SBR LATEX |
viscosity | 100-300 |
Solid Content | 49-50 |
PH | 7.5-8.5 |
MFFT | 58 |
Film Hardness | Hard |
heat forming textiles , excellent water resistant , dipping and back coating technic
Chemistry | X-SBR LATEX |
viscosity | 50-300 |
Solid Content | 49-50 |
PH | 6.5-7.5 |
MFFT | >0 |
Film Hardness | soft |
high filer load ability,highly flexible and good adhesion to fibers of artificial grass
Our products HaveNo serious damage on the environment
our material has no containers handling problem Keep it from freezing and sunlight between 5 to 35C˚
Expiry date of this product : at least six months, Keep it in appropriate indoor warehouse.
REGULATION (EC) No 1272/2008 OF THE EUROPEAN PARLIAMENT AND OF THE COUNCIL of 16 December 2008 on classification, labelling and packaging of substances and mixtures, amending and repealing Directives 67/548/EEC and 1999/45/EC, and amending Regulation (EC) No 1907/2006